Mediante la prueba heat soak según la norma EN 141791, el vidrio se somete durante un espacio mínimo de 4 horas a una temperatura de 290 °C para transformar las inclusiones de sulfuro de níquel y evitar una posterior rotura espontánea de la plancha de vidrio. | During a Heat Soak Test in accordance with EN 14179-1 the panes are exposed to a temperature of 290 °C for at least four hours in order to transform nickel sulfide inclusions and hence to prevent the pane from breaking spontaneously later. |